Atomically-thin WO3/TiO2 heterojunction for supercapacitor electrodes developed by atomic layer deposition
Composite Communications
Z. Hai, M. Karbalaei Akbari, C. Xue, H. Xu, E. Solanod, C. Detavernier, J. Hu and S. Zhuiykov